Grade |
Metal(%) |
Average size ( μ m) |
Min through 325mesh (%) |
Max moisture(%) |
Solvent |
|
LX-4000 |
72 |
40 |
9 8.0(200 mesh) |
0.15 |
MS/HA |
|
LX-4306 |
66 |
27 |
99 |
0.15 |
MS/HA |
|
LX-4308 |
6 5 |
16 |
99.5 |
0.15 |
MS/HA |
|
LX-4308P |
65 |
15 |
99.9 |
0.15 |
MS/HA |
|
LX-4310 |
65 |
28 |
99.9 |
0.15 |
MS/HA |
|
LX-4310A |
72 |
27 |
99 |
0.15 |
MS/HA |
|
LX-5122 |
72 |
30 |
99.9 |
0.15 |
MS/HA |
|
LX-5180 |
72 |
24 |
99.9 |
0.15 |
MS/HA |
|
LX-5182 |
72 |
42 |
98.5 |
0.15 |
MS/HA |
|
LX-5500 |
75 |
19 |
99.9 |
0.15 |
MS/HA |
|
LX-5500A |
72 |
19 |
99.5 |
0.15 |
MS/HA | |
| Note: MS=Mineral Spirit, HA= High boil point Aromatic solvent |
| Characteristics and Applicantions |
| Applicantions: |
These standard fineness non-leafing pastes are used where a white,brighter and highly sparkling metallic effect finish is desired.They are suitable for interior and exterior paints and high quality industrial coatings.
|
| |
|
| Pre-disperse: |
Place enough thinner into aluminum paste in proportion with 1:2, stir them carefully, adding resin, organic solvent and additive when no grain or particle exists. |
| |
|
| Notice: |
Avoid using milling equipment to disperse aluminum paste, since they would destroy interior struture. Aluminum paste must be isolated with water, acid and base,seal the container cover soon after using it. | |
|
|
|